Home
 
  advanced search>

Home
/ Automotive / Publications /
DUAL-TEN® Brochure  

DUAL-TEN® Brochure - Forming Limits

back  |  next 


As shown in Figure 5, the ASM standard shape of the forming limit curve for steel can be used for DUAL-TEN® steel, and the equation for the FLC calculation using n-value and sheet thickness is still valid for DUAL-TEN® steel.  The n-value used for the FLC calculation should be determined from stress and strain data from 10% strain to end of uniform elongation.

Forming Limit Diagram for DUAL-TEN(TM) 600/590 AND DUAL-TEN(TM) 780/800
Figure 5: The Experimentally Determined Forming Limit Diagram for DUAL-TEN® 600/590 steel and DUAL-TEN® 780/800 steel [4] 


back  |  next 

 

Copyright 2010 United States Steel.  All rights reserved. Site feedback.
Please see our Legal Notice for conditions regarding the use of this site and links provided to third-party Web sites.
Trademarks and Ownership